SAE AIR5065A

Influence of Grain Flow on Bolt Integrity (Stabilized: May 2012)

SAE International , 05/09/2012

$47.00 $94.00
This document has been declared "Stabilized" and will no longer be subjected to periodic reviews for currency. Users are responsible for verifying references and continued suitability or technical requirements. New technology may exist.

Performed tensile and fatigue tests on bolts to determine if cutting of materials flow lines at the bolt underhead would degrade bolt integrity. Five different alloys used in aerospace industry fatigue critical applications were employed to fabricate 5/16 to « inch diameter bolts. These bolts were machined from bar stock producing fully cut material flow lines under their heads. Tensile testing with and without underhead washers was performed along with industry standard fatigue testing.

Product Information

Published: 05/09/2012
File Size: 1 file , 320 KB
Language: English
Note: This product is unavailable in Ukraine, Russia, Belarus
SAE AIR5065A
SAE AIR5065A

$47.00

SAE AIR 5065
SAE AIR 5065