API RP 5L3:1996

Recommended Practice for Conducting Drop-Weight Tear Tests on Line Pipe

American Petroleum Institute , 01/01/1996

$70.00 $140.00
Describes procedures for a recommended method for conducting drop-weight tear tests to measure the fracture appearance or fracture ductility of line pipe as referenced in API Specification 5L.

Product Information

Published: 01/01/1996
Pages: 9
File Size: 1 file , 960 KB
Language: English
Note: This product is unavailable in Russia, Cuba, Syria, North Korea, Ukraine, Belarus, Iran
API RP 5L3 (R2020)
API RP 5L3:1996

Related Documents

API MPMS Chapter 10.1:2002
API Publ 4723:2002
API 570:1998
API 570:1998

$72.00