BS 3473-1:1991

Chemical resistance of glass used in the production of laboratory glassware-Method for determination of resistance of glass to attack by a boiling aqueous solution of mixed alkali

BSI Group , 07/31/1991

$80.00 $160.02
Method and classification for resistance to attack by boiling aqueous sodium carbonate and sodium hydroxide solution. Cross References:BS 970:Part 1BS 2092BS 3473:Part 2BS 3473:Part 3BS 3473:Part 4BS 3978BS 5922 BS 6523Health and Safety at Work etc. Act 1974